Cambridge low-carbon and self-healing concrete blocks assessed after six years in a Dyson Building wall
Two hundred lightweight blocks in a Cambridge plantroom wall were surveyed after six years; the self-healing additives showed no detectable adverse effect on the host concrete.

Researchers at the University of Cambridge have reported six-year in-service results for low-carbon and self-healing lightweight concrete blocks in the journal Case Studies in Construction Materials. Two hundred full-size blocks (400 mm × 215 mm × 100 mm; 100 per family) were hand-manufactured in the university laboratory. With the contractor Morgan Sindall, they were installed in a non-structural internal plantroom wall of the James Dyson Building sciencedirect.com
Case Studies in Construction Materialssciencedirect.comOpen source ↗. The paper reports 30 mixes: 23 low-carbon and 7 self-healing.
Binders, additives and test methods
The low-carbon binders were PC–GGBS–MgO blends and slag-rich binders activated with reactive MgO, lime and/or sodium carbonate. The self-healing mixes used sodium silicate microcapsules, expansive minerals or PVA-coated MgO pellets. All mixes contained Lytag lightweight aggregate.
Cube strengths were measured at 7 and 28 days and, for selected mixes, at 240 days. After six years the installed blocks were surveyed with a rebound hammer, ultrasonic pulse velocity (UPV), surface resistivity and Torrent air permeability. The results were interpreted as relative indices against the control of each family.
Six-year results and embodied carbon
The rebound indices of the alkali-activated mixes fell within a narrow band of 0.58–0.73 × that of the PC control. Those of all self-healing mixes were within about 10% of their control sciencedirect.com
Case Studies in Construction Materialssciencedirect.comOpen source ↗. Most mixes gave UPV values within the scatter of their controls.
PC-free slag mixes activated only by MgO and/or lime showed markedly higher air permeability, which the authors attribute mainly to weak slag activation. The self-healing mixes gave UPV, resistivity and air-permeability indices similar to those of their control. According to the authors, this indicates no detectable adverse effect of the healing additives on the host concrete in this sheltered exposure.
The binder embodied carbon of the slag-rich and clinker-free mixes was 45–85 kgCO₂e/m³, which is 69–83% below that of the PC control. At block level, with the Lytag aggregate included, the reduction was 36–44%. The authors also discuss the challenges of scale-up and of interpreting non-destructive test data for lightweight concrete blocks.